Submit PaperPapers tagged with "Casting Defects"
CASTING DESIGN AND SIMULATION OF QRL CYLINDER FOR DEFECT MINIMIZATION USING AUTOCAST SOFTWARE
Metal Casting Is A Dominating Field Of Production Processes Used To Produce Mechanical Parts Of Complex Shape And Size. It Is Always Considered As A Backbone Of Production Industry. The Paper Covers The Detailed Analysis Carried Out To Redu...
AN OPTIMIZATION OF PROCESS PARAMETERS: TO MINIMIZE THE CASTING DEFECTS OF MILD STEEL PRODUCT IN GREEN SAND CASTING PROCESS BY USING ORTHOGONAL ARRAY AND TAGUCHI METHOD
The Main Purpose Of This Paper Is To Reduce The Casting Defects By Analyzing And Detecting With The Use Of Non-destructive Testing Methods. In Most Of The Industries As We All Are Aware About The Normal Casting Defects Which Are Generated D...
AN OPTIMIZATION OF PROCESS PARAMETERS: TO MINIMIZE THE CASTING DEFECTS OF MILD STEEL PRODUCT IN GREEN SAND CASTING PROCESS BY USING ORTHOGONAL ARRAY AND TAGUCHI METHOD
The Main Purpose Of This Paper Is To Reduce The Casting Defects By Analyzing And Detecting With The Use Of Nondestructive Testing Methods. In Most Of The Industries As We All Are Aware About The Normal Casting Defects Which Are Generate...