Impact Factor: 7.883
Submit Paper
Volume 6, Issue 12 (December 2020)

Surface Analysis And Mechanical Behaviour Of Polysiloxane Coating On Alloy Steel Substrate

Impact Factor
7.883
Call For Paper
Volume 12 Issue 10

October 2026

Download Paper Format
Copyright Form
Share on:

Author(s)

M. Sivamanikandan K. Saravanan

Abstract

This Project Deals About Developing Anti-scratch Coating For Automotive Body. Automobiles Undergo Severe Scratches On Body And To Some Extend On The Wind Shields. An Experimental Investigation Is Carried Out Over Automotive Body To Improve The Scratch Res


Keywords

Substrate Coating Spray Coating Polysiloxane Coating Optical Microscope SEM Vickers’s Hardness Test.