Srikanth K Sowrabh R Shetty Vinit Paul Mohammed Ibrahim, Guide: Dr. N Jegadeeswaran

Abstract

In Gas Turbines, Surface Degradations Such As Hot Corrosion Occur At Places Like Turbine Blades, Tubes Etc. Where The Temperature Is High. The Turbines Become Less Effective And Noisy Because Of These Defects. The Present Study Is On High Velocity Oxy-Fue


Keywords

Hot Corrosion High Velocity Oxy Fuel Thermogravimetric Analysis XRD SEM